Nanoindenter – KLA Instruments iMicro Nanoindenter

The KLA iMicro Nanoindenter is designed for nanoscale indentation hardness testing on a variety of materials including soft polymers, thin films and hard coatings. The optional NanoBlitz 3D feature provides material hardness, modulus and stiffness property maps.
 

Location: University Instrumentation Center, University of New Hampshire, Durham NH

Manufacturer: KLA Corporation

Link to Webpage

Contact: John Wilderman
John.Wilderman@unh.edu